Nanoindentation_CuZn23Si2.5_IMWS

hardness and modulus

Data and Resources

  • FEMBau02_CuZn23Si2_5.opju

    Explore
    • More information
    • Download
  • FEMBau02_CuZn23Si2_5_modulus Graph.pngPNG